Correlation between microstructure and creep behavior in liquid-phase-sintered α-Silicon Carbide
(The American Ceramic Society, 2006)
The influence of increasing the sintering time from 1 to 7 h on the microstructure evolution and the mechanical properties at high temperature was studied in α-silicon carbide (α-SiC) sintered in argon atmosphere with ...
A critical assessment of the dislocation-driven model for superplasticity in yttria tetragonal zirconia polycrystals
(The American Ceramic Society, 2008)
In this paper, the origin of the threshold stress in pure 3 mol %-yttria tetragonal zirconia polycrystals (YTZP) is analysed in detail. At this regard, the two explanations reported in literature are discussed thoroughly. ...
α-Al2O3 sapphire and rubies deformed by dual basal slip at intermediate temperatures (900–1300 °C): I. Dislocation organization
(Elsevier, 2009)
Under a load orientation that hinders twinning and impedes fracture, sapphire and Cr-doped α-Al2O3 single crystals (rubies) were deformed from 1500 °C to slightly above the brittle to ductile transition temperature of 900 ...
Effect of atmosphere and sintering time on the microstructure and mechanical properties at high temperatures of alpha-SiC sintered with liquid phase Y2O3-Al2O3
(Elsevier, 2006)
The influence that the atmosphere (N2 or Ar) and sintering time have on microstructure evolution in liquid-phase-sintered α-SiC (LPS-α-SiC) and on its mechanical properties at high temperature was investigated. The ...
α-Al2O3 sapphire and rubies deformed by dual basal slip at intermediate temperatures (900–1300 °C): II. Dissociation and stacking faults
(Elsevier, 2009)
Sapphire and rubies (undoped and Cr-doped α-Al2O3 single crystals) have been deformed in compression at temperatures lower than those previously used in studies of dislocations in the basal slip plane. Above 1400 °C, several ...
Tensile deformation and fracture mechanisms of Cu/Nb nanolaminates studied by in situ TEM mechanical tests
(Elsevier, 2018)
The mechanisms of deformation and failure of Cu/Nb nanolaminates manufactured by accumulated roll bonding were analysed using in-situ TEM mechanical tests. Dog-bone small-scale tensile specimens were prepared using a ...
High temperature internal friction in a Ti–46Al–1Mo–0.2Si intermetallic, comparison with creep behaviour
(Elsevier, 2016)
Advanced γ-TiAl based intermetallics Mo-bearing have been developed to obtain the fine-grained microstructure required for superplastic deformation to be used during further processing. In the present work we have studied ...
Effect of the heat treatment on the mechanical properties and microstructure of Scalmalloy® manufactured by Selective Laser Melting (SLM) under certified conditions
(Elsevier, 2023)
Mechanical properties and microstructure of Scalmalloy® processed by Selective Laser Melting (SLM) under certified conditions are studied. Two types of samples are considered: as-built and heat-treated at 325 °C for 4 h. ...